Zinc cladding
Showing results 1-8 of 8
Zinc cladding – white corrosion on zinc panels
-
Lack of cleaning/rainwashing
-
Salt deposits
Zinc cladding – dents/impact damage
-
Stones, balls, vehicles
-
Sheets damaged during installation
Zinc cladding – uneven colour
-
Parts of the wall area are more exposed to the weather or rainwashing that slows the development of the traditional zinc oxide on the surface
Zinc cladding – small holes appearing in the zinc
-
Condensation forming on the back of the zinc panels – pure water is very damaging to zinc
-
Corrosion initiated through the use of the wrong fixings
-
The zinc is not isolated from the plywood substrate
-
CCA (copper-based) treated plywood was used
Zinc cladding – buckling
-
Thermal movement in a panel that is restricted at panel ends
-
Interlocking panel movement restricted because joints are fitted too tightly
-
Sliding clips not allowing movement
Zinc cladding – dirt build-up
-
Lack of rainwashing
Zinc cladding – fingerprints
-
Oil from the skin left on the surface of the zinc
Zinc cladding – scratches
-
Scratched during installation or by occupants working in the vicinity of the zinc
-
Scratched by plants