Texture-coated fibre-cement – vertical cracking at sheet joints

Texture-coated fibre-cement – horizontal cracking

Stucco – random hairline cracking

Stucco – coating failure

Hairline cracking in EIFS

Distortion of uPVC door and window frames

Moisture in sealed insulating glass units

  • Edge seal damage or failure due to UV light, moisture in window frame, wind deflection 

    How to repair

  • Damage caused during installation; manufacturing defect

    How to repair

Cavity brick or concrete block veneer – cracks in mortar

  • Differential settlement of the building caused by swelling/shrinking of clay soils, inadequate foundations or tree roots under the foundations, and indicated by cracks in the mortar stepped across the face of the wall

    How to repair

  • Soil load behind basement wall causing deformation

    How to repair

  • View all repairs

Cavity brick or concrete block veneer – cracks in bricks

  • Differential settlement of the building caused by swelling/shrinking of clay soils, inadequate foundations or tree roots under the foundations, and indicated by cracking through the bricks 

    How to repair

  • Soil load behind basement wall causing deformation

    How to repair

  • View all repairs

Cracks in the mortar and/or bricks

  • No control joints incorporated in wall

    How to repair

  • Differential settlement of the building caused by swelling/shrinking of clay soils and inadequate foundations and indicated by cracking through the mortar stepped across the face of the wall

    How to repair

  • View all repairs

Concrete blockwork – cracks in the mortar and/or blocks

  • No control joints incorporated in wall

    How to repair

  • Differential settlement of the building caused by swelling/shrinking of clay soils and inadequate foundations and indicated by cracking through the mortar stepped across the face of the wall

    How to repair