Rust on zinc/aluminium or aluminium/zinc alloy-coated steel roofing
-
Erosion of or scratching damage to the zinc/aluminium or aluminium/zinc alloy coating, exposing the steel
-
Lack of rain washing. Rain washing tends to be less effective on roofs with less than 15 degrees slope
-
Roofing metal is in contact with or has run-off from cedar or redwood, or timber treated with a copper-based preservative treatment
-
Roofing has run-off from translucent (PVC) sheeting
-
Corrosion of the steel in a corrosive environment such as near a swimming pool, or in coastal, industrial or geothermal regions
-
Inadequately primed end and/or side laps
-
Use of lead flashings
-
The roofing is near the end of its serviceable life
Rust on alloy-coated pre-finished steel roofing
-
Paint failure and subsequent erosion of or scratching damage to the zinc/aluminium or aluminium/zinc alloy coating, exposing the steel
-
Roofing material is in contact with or has run-off from cedar or redwood, or timber treated with a copper-based preservative treatment
-
The roofing has run-off from translucent (PVC) sheeting
-
The roofing is near the end of its serviceable life
Zinc roofing – white surface corrosion
-
Lack or rainwashing. Rain washing tends to be less effective on roofs with less than 15 degrees slope
-
The roofing material is in contact with, or has run-off from, cedar or redwood, or timber treated with a copper-based preservative treatment
-
The roofing has run-off from translucent (PVC) sheeting
Corrosion: red rust on galvanised mild steel cladding
-
Galvanised coating has eroded to expose bare metal
-
Profiled metal cladding is in contact with or has run-off from cedar or redwood, or timber treated with copper-based preservative treatment
-
Galvanised mild steel cladding has run-off from translucent sheeting (PVC), glass, pre-painted roofing, glazed tiles, unpainted zinc/aluminium alloy-coated mild steel or aluminium
-
Damage to the galvanised coating during fixing exposing steel
-
Exposure to a corrosive environment such as a swimming pool, or in coastal, industrial or geothermal areas
-
Inadequately primed end and/or side laps
-
Cladding in ground contact
-
Insufficient rain washing
Red rust on zinc/aluminium or aluminium/zinc alloy-coated steel
-
Corrosion of the steel when zinc/aluminium alloy coating has eroded to expose the steel
-
Cladding material in contact with or has run-off from cedar or redwood, or timber treated with a copper-based preservative treatment
-
Cladding has run-off from translucent (PVC) sheeting
-
Corrosion of the steel in a highly corrosive environment such as a swimming pool, or in coastal, industrial or geothermal regions
-
For factory coated material, wrong coating specification for the in-use conditions
-
Inadequately primed end and/or side laps
-
Cladding in ground contact
-
Insufficient rain washing