Stucco
Showing results 1-12 of 13
Rust stains on stucco
-
Hairline cracking in the stucco admitting moisture causing corrosion of the reinforcing mesh
Impact damage to stucco
-
Stones, balls, vehicles
Stucco – drummy plaster
-
Loss of bond between the plaster coats
-
Plaster shrinkage
-
Poor initial application of plaster
Stucco – sealant cracking at movement control joint
-
UV exposure
-
Sealant not suitable for being painted
-
Too much movement for the grade of sealant
-
Sealant not installed over a backing rod or bond breaker tape
-
Sealant at the end of its serviceable life
Stucco – random hairline cracking
-
Shrinkage as a result of incorrect plaster mix and/or inadequate curing
-
Excessive trowelling during application
-
No movement control joints installed
-
Building movement or settlement
-
Building subjected to vibration movement such as earthquake, high wind
Stucco – horizontal or diagonal surface cracking
-
No movement control joints or poorly located movement control joints installed
-
No additional reinforcing at corners of openings
-
Poor application of texture coating
-
Insufficient or a too large separation between reinforcing and backing
-
Building movement or settlement
-
Framing shrinkage
-
Building subjected to vibration movement such as earthquake, high wind
Stucco – chalking paint
-
Weathering, UV light exposure – chalking will be more visible with darker colours
Stucco – fading paint
-
Weathering, UV light exposure – darker colours are more prone to fading
Stucco – coating failure
-
Lack of maintenance
-
Paint at end of serviceable life
-
Moisture levels in substrate too high when initially plastered
-
Moisture getting into the plaster through hairline cracking
-
Paint unsuitable to be used with cement-based plaster
-
Building subjected to vibration movement such as earthquake, high wind
Stucco – too close to or in ground contact
-
Installed too close to the ground
-
Gardens have been built up
-
Path or paving laid against the cladding
Leaking through stucco
-
Cracks in the cladding systems
-
Paint or sealant failure
-
No cap or saddle flashings at junctions of parapet and balcony walls
-
Junctions with other claddings and/or roof poorly detailed/constructed
-
Omission of head flashings to doors/windows
-
Minimal jamb flange cover of aluminium windows
Straw bale construction – moisture entry in walls
-
Inadequate eaves protection and wind-driven rain striking walls
-
Too much reliance on stucco plaster finish as waterproofing
-
Deteriorating plaster finish no longer adequately protects walls
-
Poor or no damp-proof membrane
-
Lack of ground clearance